CIMENT GROUT, WATER PROOFING, WEBER
- New concrete should be cured for at least 28 days and should have a pull off strength ≥ 1.5 N/mm².
- Cement or mineral based substrates must be prepared mechanically using abrasive blast cleaning or scarifying equipment to remove cement laitance and to achieve an open textured surface.
More Details...
wo-component with latex cementitious coating, which can be simply achieved by mixing a prepacked powder with a formulated admixture, and subsequent painting the slurry on various substrates. It protects a wide range of buildings and structural concrete components with excellent resistance to water, long-term weathering and scratching.
More Details...
- Concrete, Cement-Sand Render / Screed & Masonry surface must be fully cured, dry, sound, flat or true & free of contaminants eg. grease, oil, dust, loose particles, laitance etc.
- Steel / Metal surface must be free of scales, rust, grease, oil etc.
- Damp the surface before coating and sweep the excess water to avoid ponding on the horizontal area.
More Details...